To meet the challenge of regenerating bone lost to disease or trauma, biodegradable scaffolds are being investigated as a way to regenerate bone without the need for an auto- or allograft. Here, we have developed a novel microsphere-based chitosan/nanocrystalline calcium phosphate (CaP) composite scaffold and investigated its potential compared to plain chitosan scaffolds to be used as a bone graft substitute. Composite and chitosan scaffolds were prepared by fusing microspheres of 500-900 microm in diameter, and porosity, degradation, compressive strength, and cell growth were examined. Both scaffolds had porosities of 33-35% and pore sizes between 100 and 800 . However, composite scaffolds were much rougher and, as a result, had 20 times more surface area/unit mass than chitosan scaffolds. The compressive modulus of hydrated composite scaffolds was significantly higher than chitosan scaffolds (9.29 +/- 0.8 MPa vs. 3.26 +/- 2.5 MPa), and composite scaffolds were tougher and more flexible than what has been reported for other chitosan-CaP composites or CaP scaffolds alone. Using X-ray diffraction, scaffolds were shown to contain partially crystalline hydroxyapatite with a crystallinity of 16.7% +/- 6.8% and crystallite size of 128 +/- 55 nm. Fibronection adsorption was increased on composite scaffolds, and cell attachment was higher on composite scaffolds after 30 min, although attachment rates were similar after 1 h. Osteoblast proliferation (based on dsDNA measurements) was significantly increased after 1 week of culture. These studies have demonstrated that composite scaffolds have mechanical properties and porosity sufficient to support ingrowth of new bone tissue, and cell attachment and proliferation data indicate composite scaffolds are promising for bone regeneration.
Degree of deacetylation (DDA) and molecular weight (MW) of chitosans are important to their physical and biological properties. In this study, two chitosans, HS (DDA = 73.3%) and AT (DDA = 76.8%), were deacetylated with 45% sodium hydroxide under nitrogen atmosphere at 80 °C or 90 °C for up to 120 min, to obtain two series of chitosans. The polymers produced were characterized for MW by gel permeation chromatography, DDA by titration and UV-vis methods, and crystallinity, hydrophilicity and thermal stability by X-ray diffraction, water contact angle and differential scanning calorimetry respectively. Films, made by solution casting in dilute acetic acid at ambient conditions, were evaluated for biological activity by albumin adsorption and the attachment and growth of a pre-osteoblast cell line. Chitosans with between 80–93% DDA’s (based on titration) were reproducibly obtained. Even though deacetylation under nitrogen was supposed to limit chain degradation during decetylation, MW decreased (by maximum of 37.4% of HS and 63.0% for AT) with increasing deacetylation reaction time and temperature. Crystallinity and decomposition temperature increased and water contact angles decreased with processing to increase DDA. Significantly less albumin was absorbed on films made with 93% DDA chitosans as compared with the original materials and the AT chitosans absorbed less than the HS chitosans. The cells on higher DDA chitosan films grew faster than those on lower DDA films. In conclusion, processing conditions increased DDA and influenced physicochemical and biological properties. However, additional studies are needed to unambiguously determine the influence of DDA or MW on in vitro and in vivo performance of chitosan materials for bone/implant applications.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.