The effects of the addition of 0.29 wt % Ce on the recrystallization behavior of an Al–Cu–Li–0.13Zr (wt %) alloy during isothermal annealing were investigated. Ce addition greatly improved inhibition of recrystallization in this alloy compared with that in the Ce-free alloy. The texture of the Ce-containing alloy contained a large amount of β-fibers and fibrous unrecrystallized grain microstructures distributed along the rolling direction in the overall annealing process. The improved recrystallization resistance endowed by Ce addition can be attributed to the large number of small Al8Cu4Ce species formed on the grain boundary. These fine particles with high-temperature stability can exert a Zener pressure on the Al3Zr dispersoid-free grain boundary. The yield strength of the Ce-containing alloy increased significantly, to 38 MPa, and the fracture toughness improved by 56.28% compared with those of the Ce-free alloy. This work provides a convenient and economical method for enhancing the overall performance of an Al–Cu–Li–Zr alloy via recrystallization inhibition by Ce addition.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.