Pressure-induced phase transitions of multiferroic BiFeO 3 have been investigated using synchrotron radiation X-ray diffraction with diamond anvil cell technique at room temperature. Present experimental data clearly show that rhombohedral (R3c) phase of BiFeO 3 first transforms to monoclinic (C2/m) phase at 7 GPa, then to orthorhombic (Pnma) phase at 11 GPa, which is consistent with recent theoretical ab initio calculation. However, we observe another peak at 2θ=7° in the pressure range of 5-7 GPa that has not been reported previously. Further analysis reveals that this reflection peak is attributed to the orthorhombic (Pbam) phase, indicating the coexisting of monoclinic phase with orthorhombic phase in low pressure range. Keywords:BiFeO 1.INTRODUCTIONMultiferroics, which exhibit both ferroelectric and magnetic order in the same phase, have attracted great interests because of these unique properties [1,2]. Especially, the magnetic properties of multiferroics can be modulated by external electric fields and vice versa. Bismuth ferrite, BiFeO 3 (BFO) as a prototype multiferroic material, is perhaps the only compound with both magnetic and ferroelectric at ambient conditions [3,4]. In BFO, the 6s 2 lone pair electrons of Bi 3+ arouse the ferroelectricity until the temperature reaches T C =1100 K [5]. Spiral spin cycloid modulated G-type antiferromagnetic order with a periodicity of 62 nm occurs below the Neel temperature (T N =640K) [5,6]. Due to these promising physical properties, many experimental and theoretical efforts have been devoted to its structural characteristics [7] and the nature of magnetoelectric coupling [8,9]. At ambient conditions, BFO crystallizes in the rhombohedral structure with R3c (Z=161) space group, with c-axis parallel to the diagonals of the perovskite cube [10]. The Fe 3+ ion is coordinated by six oxygen atoms, forming an octahedral FeO 6 . Research of phase transitions under high pressures of BFO has been of long-standing interest [3,7,11,12]. Early literature has reported that no phase transition occurs in BFO until the high pressure reaches up to 70 GPa [13]. In contrast, some studies have demonstrated that BFO has undergone several structural phase transitions during the upstroke process. At high pressure above 10 GPa, Haumont et al.[12] and Guennou et al. [14] found that BFO transforms to the orthorhombic Pnma structure instead of others. While at low pressure, BFO exhibits a variety of phase transitions. For instance, by using x-ray diffraction (XRD) and far-infrared spectroscopy, Haumont et al. [12] found that BFO remains the rhombohedral structure up to 6.2 GPa, then changes to a monoclinic structure with space group C2/m. Nevertheless, in a more recent study, a phase transition from the polar rhombohedral R3c phase to the antipolar orthorhombic Pbam phase with antiferroelectric character of atomic displacements has been revealed at 3 GPa by using neutron powder diffraction [15]. Furthermore, Guennou et al. [14] have reported that three different phase transitio...
In the last few years, Nd3+ doped fluoride crystals have achieved some amazing laser performances by codoping buffer ions such as Y3+ and Gd3+ ions, which lead to the changing of local structure of Nd3+ ions. In this work, effects of doping concentration of Gd3+ and Y3+ ions on optical properties are discussed. The relationships between spectroscopic properties and the unit cells are also discussed. Nd, Y:CaF2 and Nd, Gd:CaF2 disordered crystals are grown by using temperature gradient technique (TGT). Among 0.5 at.%Nd, x at.%Gd(x=2, 5, 8, 10):CaF2 crystals, the crystal with Gd3+ of 2 at.% has the longest fluorescence lifetime (499 s). Increasing the concentration of Gd3+ up to 5 at.%, the crystal has a maximum absorption cross section of 1.910-20 cm2, and a maximum emission cross section of 1.910-20cm2. The crystal with Gd3+ of 8 at.%has a maximum emission bandwidth of 29.03 nm(FWHM). Among 0.6 at.%Nd, x at.%Y(x=2, 5, 8, 10):CaF2 crystal, the crystal with Y3+ of 5 at.%has the biggest absorption cross section (2.4110-20 cm2), and the biggest emission cross section (3.1710-20 cm2), when the concentration of Y3+ is 5 at.%. When the Y3+ concentration increases up to 10 at.%, the crystal has a longest fluorescence lifetime of 359.4 s and maximal emission bandwidth of 26 nm(FWHM).The different concentrations of codoping ions have different effects on the Nd:CaF2 crystals, for the formations of different optical centers. In order to study the effects of local structure around Nd3+ on the optical properties in a set of Nd:CaF2 single crystals with different codoping concentrations of Gd3+ and Y3+, the unit cell parameters are investigated by X-ray diffraction. With different concentrations of Gd3+ and Y3+ ions in Nd:CaF2 crystal, the local structure of Nd3+ changes, which leads to different optical properties. The relevant details will further be explained in this paper.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.