2014
DOI: 10.1016/j.electacta.2013.12.124
|View full text |Cite
|
Sign up to set email alerts
|

Accurate Electrochemical Measurement of Magnesium Corrosion Rates; a Combined Impedance, Mass-Loss and Hydrogen Collection Study

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

21
426
1

Year Published

2014
2014
2022
2022

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 541 publications
(448 citation statements)
references
References 53 publications
21
426
1
Order By: Relevance
“…2(a) and (b), which present typical EIS data for Mg corrosion containing an inductive loop, from Qiao et al [3], for Mg specimen 19 (in the notation of Qiao et al [3]) immersed at the open circuit potential in 3.5% NaCl solution saturated with Mg(OH) 2 at 25 °C, for which there was significant micro-galvanic corrosion as evidenced by the corrosion morphology. The definitions of R s , R t , and R P , follow that in King et al [1]. R s is the solution resistance, R t is the charge transfer resistance, and R P is the polarisation resistance.…”
Section: Introductionmentioning
confidence: 99%
See 4 more Smart Citations
“…2(a) and (b), which present typical EIS data for Mg corrosion containing an inductive loop, from Qiao et al [3], for Mg specimen 19 (in the notation of Qiao et al [3]) immersed at the open circuit potential in 3.5% NaCl solution saturated with Mg(OH) 2 at 25 °C, for which there was significant micro-galvanic corrosion as evidenced by the corrosion morphology. The definitions of R s , R t , and R P , follow that in King et al [1]. R s is the solution resistance, R t is the charge transfer resistance, and R P is the polarisation resistance.…”
Section: Introductionmentioning
confidence: 99%
“…The EIS data analysis proposed by King et al [1] can be understood from Figs. 2(a) and (b), which present typical EIS data for Mg corrosion containing an inductive loop, from Qiao et al [3], for Mg specimen 19 (in the notation of Qiao et al [3]) immersed at the open circuit potential in 3.5% NaCl solution saturated with Mg(OH) 2 at 25 °C, for which there was significant micro-galvanic corrosion as evidenced by the corrosion morphology.…”
Section: Introductionmentioning
confidence: 99%
See 3 more Smart Citations