2018
DOI: 10.1016/j.ijbiomac.2017.11.167
|View full text |Cite
|
Sign up to set email alerts
|

Analysis of lecithin treatment effects on the structural transformation of wool fiber using vibrational spectroscopy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
5
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
7
1

Relationship

1
7

Authors

Journals

citations
Cited by 21 publications
(5 citation statements)
references
References 20 publications
0
5
0
Order By: Relevance
“…Wool-MOF comprises characteristic peaks of wool related to the peptide bond including amide A at 3374 cm -1 and amide B at 3068 cm -1 ascribed to N-H stretching vibrations along with amide I at 1650 cm -1 , amide II at 1519 cm -1 and amide III at 1238 cm -1 [46,47]. All of these confirm the nucleation of Zr-MOF onto the surface of wool.…”
Section: Fourier Transform Infrared Spectroscopymentioning
confidence: 57%
“…Wool-MOF comprises characteristic peaks of wool related to the peptide bond including amide A at 3374 cm -1 and amide B at 3068 cm -1 ascribed to N-H stretching vibrations along with amide I at 1650 cm -1 , amide II at 1519 cm -1 and amide III at 1238 cm -1 [46,47]. All of these confirm the nucleation of Zr-MOF onto the surface of wool.…”
Section: Fourier Transform Infrared Spectroscopymentioning
confidence: 57%
“…In addition, a new characteristic peak appeared at 669 cm −1 in the spectrum of the treated fibers. According to the literature, this peak was mainly caused by the stretching vibration of the C–S bond [ 40 ]. The increase in C–S bond content may be related to the destruction of disulfide bonds and the formation of sulfonate radicals.…”
Section: Resultsmentioning
confidence: 99%
“…The peak is associated with CH 2 bending mode and not affected by other factors. 29 The ratio of disulphide bond intensity (511 cm −1 ) to intensity of the peak located at 1451 cm −1 can reflect the disulphide bonds concentration in wool. 30 After calculations were done, results indicated that the ratio of the raw wool (1.3) was higher than that of the modified wool (1.1).…”
Section: Disulphide Bond Analysismentioning
confidence: 99%