Analyzing the nanoindentation response of carbon black filled elastomers

Abstract: Carbon black (CB) filled elastomers are structurally complex materials that offer unique properties at different length scales. They have tremendous potential applications in a number of fields including the automotive and aerospace industries and for designing innovative smart materials such as artificial muscles but their applications remain limited primarily due to inadequate understanding of their unique mechanical properties. Here, using the Berkovich technique to probe the surface mechanical properties a… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4

Relationship

1
3

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 40 publications
0
1
0
Order By: Relevance
“…17 The additional physical crosslinks hinder to some extent the relative displacement of the chain segments which are required for the nuclei formation and growth. 29,35,36…”
Section: Resultsmentioning
confidence: 99%
“…17 The additional physical crosslinks hinder to some extent the relative displacement of the chain segments which are required for the nuclei formation and growth. 29,35,36…”
Section: Resultsmentioning
confidence: 99%