The growth of Nd 3+ doped lithium niobate crystals using Bridgman method has been reported in this paper. By means of the optimum conditions such as proper feed materials, sealed platinum crucibles, growth rate of 1-1⋅5 mm/h and temperature gradient of 30-35°C/cm across the solid-liquid interface under the furnace temperature of 1300°C, single crystals containing Nd 3+ ion with 0⋅54 mol% concentration were obtained. X-ray diffraction and ICP-AES were used to characterize the crystals and its composition. The absorption, emission and fluorescence lifetime are also measured. Based on the Judd-Ofelt theory, we obtained the optical parameters of the crystal such as the luminescent quantum efficiency, the radioactive lifetimes, the branching ratios and the emission cross-section.