Burst Ductility of Zirconium Clads: The Defining Role of Residual Stress

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 10 publications
(1 citation statement)
references
References 49 publications
0
1
0
Order By: Relevance
“…the goniometer with head, with Vantec TM area detector and appropriate video plus laser tracking. Measured, at the centre of the tube cross-section using standard d-sin 2 Ψ 17,18 .Residual stress is measured at Fusion zone of weld material; of the lateral surface on weld samples, for calculation 19 of the residual stress, the following Equation-2 is used.…”
Section: Experimental Workmentioning
confidence: 99%
“…the goniometer with head, with Vantec TM area detector and appropriate video plus laser tracking. Measured, at the centre of the tube cross-section using standard d-sin 2 Ψ 17,18 .Residual stress is measured at Fusion zone of weld material; of the lateral surface on weld samples, for calculation 19 of the residual stress, the following Equation-2 is used.…”
Section: Experimental Workmentioning
confidence: 99%