Calcined Coke Round Robin 19 and the Precision of Bulk Density Tests

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2014
2014
2022
2022

Publication Types

Select...
3
1

Relationship

1
3

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 2 publications
0
1
0
Order By: Relevance
“…There are at least four different bulk density tests in common use by the industry, and Table II shows the ASTM D4292 VBD test. Many of these tests are strongly influenced by minor sample preparation differences, 10 which can make the comparison of results between laboratories difficult. A small amount of dedust oil (approximately 0.3 wt.%) is almost always added to CPC to reduce dusting.…”
Section: Coke Calciningmentioning
confidence: 99%
“…There are at least four different bulk density tests in common use by the industry, and Table II shows the ASTM D4292 VBD test. Many of these tests are strongly influenced by minor sample preparation differences, 10 which can make the comparison of results between laboratories difficult. A small amount of dedust oil (approximately 0.3 wt.%) is almost always added to CPC to reduce dusting.…”
Section: Coke Calciningmentioning
confidence: 99%