Ceramic composite Ti3SiC2–TiB2—Microstructure and mechanical properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
13
0

Year Published

2016
2016
2023
2023

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 22 publications
(13 citation statements)
references
References 4 publications
0
13
0
Order By: Relevance
“…The results demonstrate that Ti 3 SiC 2 decomposes to TiC and Si when the sintering temperature approached to 1000 • C [23]. Meanwhile, the Si diffused into Cu matrix and form solid solution or intermetallic compounds [24]. that Ti3SiC2 decomposes to TiC and Si when the sintering temperature approached to 1000 °C [23].…”
Section: Characterization Of Cu/ti 3 Sic 2 /C/bn/gnps Nanocompositesmentioning
confidence: 99%
See 1 more Smart Citation
“…The results demonstrate that Ti 3 SiC 2 decomposes to TiC and Si when the sintering temperature approached to 1000 • C [23]. Meanwhile, the Si diffused into Cu matrix and form solid solution or intermetallic compounds [24]. that Ti3SiC2 decomposes to TiC and Si when the sintering temperature approached to 1000 °C [23].…”
Section: Characterization Of Cu/ti 3 Sic 2 /C/bn/gnps Nanocompositesmentioning
confidence: 99%
“…that Ti3SiC2 decomposes to TiC and Si when the sintering temperature approached to 1000 °C [23]. Meanwhile, the Si diffused into Cu matrix and form solid solution or intermetallic compounds [24]. Figure 4 presents the metallographic results of composite along parallel direction to that of the compact-pressing.…”
Section: Characterization Of Cu/ti 3 Sic 2 /C/bn/gnps Nanocompositesmentioning
confidence: 99%
“…The introduction of secondary phase as reinforcement into Ti 3 SiC 2 has been proved to be an effective approach to overcome these disadvantages. For example, numerous reinforcements, including TiB 2 [9], SiC [10], c-BN [11], TiC [12], Al 2 O 3 [13] and ZrO 2 [14], have been introduced to improve the mechanical properties of Ti 3 SiC 2 . Commonly, the additions of ceramic particles can improve Vickers hardness and exural strength of Ti 3 SiC 2 matrix composites.…”
Section: Introductionmentioning
confidence: 99%
“…Commonly, the additions of ceramic particles can improve Vickers hardness and exural strength of Ti 3 SiC 2 matrix composites. For example, Górny et al [9] reported that the addition of TiB 2 could effectively improve the Vickers hardness and elastic modulus of Ti 3 SiC 2 . Tian et al [12] prepared Ti 3 SiC 2 -TiC composites and found that the Vickers hardness of the composite increased with increasing TiC content up to 90 vol.%, the exural strength was enhanced by 64% when the content of TiC was 50 vol.%.…”
Section: Introductionmentioning
confidence: 99%
“…Ti 3 SiC 2 offers advantages of heat conductivity, high electric conduction, easy processing similar to metals, oxidation resistance, light weight, and high temperature resistance, making it a useful material for multiple applications [3, 4]. Without affecting the self-lubricating properties and conductivity of copper graphite alloys, Ti 3 SiC 2 can improve the strength, hardness, and wear resistance of copper-graphite composites [5].…”
Section: Introductionmentioning
confidence: 99%