“…As shown in Figure 10(B), the open‐circuit voltage of the single cell at 600, 650, and 700°C are 1.045, 1.028, and 1.020 V, respectively. And, at 700°C, the peak power density of the single cell is about 0.75 W cm −2 , higher than other reports (0.47 W cm −2 @700°C, BZCY synthesized by Pechini method, 57 besides the cathode paste is prepared using La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 and BaZr 0.1 Ce 0.7 Y 0.2 O 3‐δ ; 0.27 W cm −2 @700°C, BZCY synthesized by SSR, 13 and BaCe 0.4 Pr 0.4 Y 0.2 O 3 is used as the positive electrode material). Figure 10(C) shows the EIS diagram.…”