2015
DOI: 10.1016/s2095-4956(15)60324-2
|View full text |Cite
|
Sign up to set email alerts
|

CO2 reforming of glycerol over La-Ni/Al2O3 catalyst: A longevity evaluative study

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

2
16
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 36 publications
(18 citation statements)
references
References 10 publications
2
16
0
Order By: Relevance
“…Nano-filament carbon with narrow hollow tube could be formed on both catalysts, Ni/Al 2 O 3 and La-Ni/Al 2 O 3 ( Figure 3c,f respectively). A long-run stability of La promoted Ni/Al2O3 catalysts for glycerol-dry reforming was proposed by Cheng et al [55]. Field emission scanning electron microscopy (FE-SEM), TEM, and HRTEM analyses of catalysts after 72 h reaction were performed, as shown in Figure 3.…”
Section: Dry Reforming Reactionsmentioning
confidence: 95%
See 2 more Smart Citations
“…Nano-filament carbon with narrow hollow tube could be formed on both catalysts, Ni/Al 2 O 3 and La-Ni/Al 2 O 3 ( Figure 3c,f respectively). A long-run stability of La promoted Ni/Al2O3 catalysts for glycerol-dry reforming was proposed by Cheng et al [55]. Field emission scanning electron microscopy (FE-SEM), TEM, and HRTEM analyses of catalysts after 72 h reaction were performed, as shown in Figure 3.…”
Section: Dry Reforming Reactionsmentioning
confidence: 95%
“…These results evidenced the role played by Zr on the carbon nanostructures, preventing the formation of fishbone carbon nanofibers during the methane decomposition process. A long-run stability of La promoted Ni/Al 2 O 3 catalysts for glycerol-dry reforming was proposed by Cheng et al [55]. Field emission scanning electron microscopy (FE-SEM), TEM, and HRTEM analyses of catalysts after 72 h reaction were performed, as shown in Figure 3.…”
Section: Dry Reforming Reactionsmentioning
confidence: 96%
See 1 more Smart Citation
“…To optimize the behavior of Ni based catalyst, La has been incorporated as a promoter for the dry reforming of glycerol [13,48,52,53]. After evaluating the effect of different content of La loaded, it was found that the glycerol conversion decreased in the order of 2%La-Ni/Al2O3 > 3%La-Ni/Al2O3 > 4%La-Ni/Al2O3 > 1%La-Al2O3 > Ni/Al2O3 > 5%La-Ni/Al2O3 > Al2O3.…”
Section: Dry Reforming Of Glycerolmentioning
confidence: 99%
“…GDR has become the focus of experimental studies only recently and the available information in the literature regarding its catalysis is rather scarce. Siew et al [17][18][19][20] studied GDR over La-promoted Ni/ Al 2 O 3 catalysts at temperatures between 650-850°C and CO 2 /G = 0-5. The authors concluded that La promotion (i) provided better metal dispersion (i.e.…”
Section: Introductionmentioning
confidence: 99%