2019
DOI: 10.1016/j.vacuum.2019.108938
|View full text |Cite
|
Sign up to set email alerts
|

Cyclic oxidation behavior of Ni3Al-basedsuperalloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 19 publications
(4 citation statements)
references
References 53 publications
0
4
0
Order By: Relevance
“…It can be seen that the pre-strain process has no significant effect on the type of oxidation product. After 5 min of oxidation, the oxidation products on both the original and pre-strained alloys are Al 2 O 3 , NiO, NiFe 2 O 4 and HfO 2 , while after 30 min of oxidation, unstable spinel NiAl 2 O 4 appears due to the reaction between Al 2 O 3 and NiO [22].…”
Section: Growth Behavior Of Short-term Oxidation Productsmentioning
confidence: 99%
See 1 more Smart Citation
“…It can be seen that the pre-strain process has no significant effect on the type of oxidation product. After 5 min of oxidation, the oxidation products on both the original and pre-strained alloys are Al 2 O 3 , NiO, NiFe 2 O 4 and HfO 2 , while after 30 min of oxidation, unstable spinel NiAl 2 O 4 appears due to the reaction between Al 2 O 3 and NiO [22].…”
Section: Growth Behavior Of Short-term Oxidation Productsmentioning
confidence: 99%
“…For instance, the outer NiO and inner Al 2 O 3 structures formed during the oxidation process of Ni 3 Al-based superalloys play a crucial role in determining the alloy's antioxidant properties [18]. In addition to applying protective layers to the matrix [19][20][21], the antioxidant properties of the alloys can be enhanced through the processes of heat treatment [8,22,23] and alloying [24,25]. These methods have achieved good results, although it is challenging to achieve further significant improvements in the antioxidant properties of superalloys.…”
Section: Introductionmentioning
confidence: 99%
“…[145] Alkaline metal, alkaline earth metal, and transition metal clusters, including Li, Na, Mg, Ag, and Ta, were also investigated (Figure 20b). [146][147][148][149][150][151][152] Ju et al studied the structure and stability of neutral and charged (FeO) n (n = 1-8) clusters using the CALYPSO code (Figure 20c) and proposed two most stable geometries, (FeO) 5 and (FeO) 4 À/þ cluster. [153] Multicomponent metal and nonmetal clusters were also widely studied.…”
Section: Clusters In Vacuummentioning
confidence: 99%
“…As one of the intermetallic compounds, Ni 3 Al has many excellent characteristics, such as low density, a high melting point, high temperature oxidation resistance, excellent creep resistance, and outstanding high temperature wear resistance [1][2][3][4]. Furthermore, it has a special abnormal phenomenon, where its yield strength increases with temperature due to its long-range ordered crystal structure of L1 2 type.…”
Section: Introductionmentioning
confidence: 99%