“…The alloys were re-melted several times to improve homogeneity. Magnetic glass-coated microwires were fabricated by the Taylor-Ulitovsky technique, which consists on drawing and casting directly from the melted Co 50 Fe 25 Si 25 alloy [26,[32][33][34][35][36][37]. The diameter of inner metallic nucleus of microwire sample is around 4.36 µm, while the diameter of external Pyrex coating is around 17.55 µm.…”