Effect of Rice Husk on Fired Ceramic Shell Strength

Abstract: In recent years, ceramic shell mould for investment casting process is often associated to defects due to its brittle properties. The defects would originate from cracking mechanism yielded from the ceramic brittleness. In this work, the improvement of ceramic shell mould by reinforcement technique was studied and analyzed. Rice husk consisting high percentage of silica content with the ability to withstand high temperature during casting process was studied as the reinforcing component as to impede cracking m… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

1
3
0

Year Published

2016
2016
2023
2023

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 11 publications
(4 citation statements)
references
References 16 publications
(12 reference statements)
1
3
0
Order By: Relevance
“…In relation to this fact, higher silica content allow the mould to be operated at higher temperature. Nonetheless, new phase of zircon (ZrSiO4) was found initiated from fused silica phase based-RH fiber as reported elsewhere [24]. Ceramic shells composition are found to be influenced by these factors and eventually enhanced their mechanical strength.…”
Section: Introductionsupporting
confidence: 67%
See 2 more Smart Citations
“…In relation to this fact, higher silica content allow the mould to be operated at higher temperature. Nonetheless, new phase of zircon (ZrSiO4) was found initiated from fused silica phase based-RH fiber as reported elsewhere [24]. Ceramic shells composition are found to be influenced by these factors and eventually enhanced their mechanical strength.…”
Section: Introductionsupporting
confidence: 67%
“…The CSm was prepared by slurry coating followed by alumina and zircon sand coating via rainfall sanding technique by sprinkle it after wax pattern immersion in the modified slurry. The steps were repeated up to 5 layers with a controlled drying and finally subjected to dewaxing and sintering for final CSm matrix consolidation [24][25][26]. The surface modification of RHs and surface fracture of composites shell mould was characterized via Scanning Electron Microscopy (SEM, Jeol JFM-6380 LA, Japan).…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…When strength of ceramic shell is not sufficient enough at high casting temperatures, there is a risk of bulging and cracking in a contact with the molten metal [4]. The mold should also be permeable to gases passing through the shell mold.…”
Section: Introductionmentioning
confidence: 99%