2018
DOI: 10.1016/j.jallcom.2017.12.045
|View full text |Cite
|
Sign up to set email alerts
|

Effect of Scandium addition on evolution of microstructure, texture and mechanical properties of thermo-mechanically processed Al-Li alloy AA2195

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
22
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 61 publications
(24 citation statements)
references
References 48 publications
2
22
0
Order By: Relevance
“…The addition of Sc increased the strength and ultimate compression strength of Mg via solid‐solution strengthening owing to its high solubility in Mg and grain refinement 4,49,50 . Also, Mg 17 Sr 2 formation enhances the mechanical properties through solid solution strengthening and precipitation hardening in Mg‐Sc‐Sr alloys due to presence of Mg 17 Sr 2 intermetallic phase 29,51 .…”
Section: Discussionmentioning
confidence: 99%
“…The addition of Sc increased the strength and ultimate compression strength of Mg via solid‐solution strengthening owing to its high solubility in Mg and grain refinement 4,49,50 . Also, Mg 17 Sr 2 formation enhances the mechanical properties through solid solution strengthening and precipitation hardening in Mg‐Sc‐Sr alloys due to presence of Mg 17 Sr 2 intermetallic phase 29,51 .…”
Section: Discussionmentioning
confidence: 99%
“…Final grain size control is the main influencing factor to enhance mechanical properties for aluminum alloys in general. Grain refinement of the third generation Al–Li alloys has been investigated by so many researchers [ 18 , [158] , [159] , [160] ]. Xinxiang et al.…”
Section: Precipitations Mechanical Properties and Grain Refinement Of...mentioning
confidence: 99%
“…Suresh et al. [ 158 ] in the investigation on effect of Sc addition on the evolution on the texture of AA2195 alloys during thermo-mechanical processing, they concluded that the Sc addition reduce the grain size and enhanced precipitation kinetics with hardness and strength improvement as well as the presence of fine Al 3 (Sc,Zr) dispersoids.…”
Section: Precipitations Mechanical Properties and Grain Refinement Of...mentioning
confidence: 99%
“…It has been demonstrated that such an addition leads to the formation of Al 3 (Sc,Zr) ternary dispersoids, resulting in a significant enhancement of the resistance to recrystallisation [19,29,43,50,51]. In a recent year, Suresh et al [52] studied the effect of Sc addition on the microstructure and mechanical properties of the hot-rolled AA2195 Al-Li alloy. In their work, the TEM image presented in Figure 6(a) showed that the majority of the particles were From Figure 7, it could be seen that the Al-Mg-Zr and Al-Mg-Zr-Sc alloys have the same hardness in the ascast state but show distinct hardening behaviours during the annealing treatment.…”
Section: Alloying With Dispersoid-forming Elementsmentioning