Effects of Sintering and Annealing Temperature on Fabrication of Transparent Lu2Ti2O7 by Spark Plasma Sintering

Abstract: Transparent lutetium titanate (Lu2Ti2O7) was fabricated by reactive spark plasma sintering. Effects of sintering and annealing temperature on the microstructure, optical and mechanical properties of Lu2Ti2O7 bodies were investigated. Pyrochlore Lu2Ti2O7 was obtained at above 1273 K and a full dense specimen was obtained above 1373 K. The average grain size increased from 0.22 to 10.85 μm up to 1773 K and abnormal grain growth occurred at 1823 K. The Lu2Ti2O7 body obtained at 1723 K for 2.7 ks for sintering and… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
21
0

Year Published

2012
2012
2022
2022

Publication Types

Select...
5
2
1

Relationship

1
7

Authors

Journals

citations
Cited by 28 publications
(21 citation statements)
references
References 21 publications
0
21
0
Order By: Relevance
“…Our main goal by choosing SPS method is to take benefit of poly-crystal made during a short time sintering, to avoid strong segregation of rare earth dopants due to lower sintering temperature than crystals, to find strong mechanical properties with small grains at a low cost [12,13]. Commercial Lu 2 O 3 (Shin-Etsu Rare Earth, Tokyo, Japan; 99.99% purity), Nd 2 O 3 (Wako Pure Chemical Co. Inc., Tokyo, Japan; 99.9% purity) and LiF (Wako Pure Chemical Co. Inc., Tokyo, Japan; 99.9% purity) powders were used as the starting materials.…”
Section: Sps Procedures At the Tohoku Universitymentioning
confidence: 99%
See 1 more Smart Citation
“…Our main goal by choosing SPS method is to take benefit of poly-crystal made during a short time sintering, to avoid strong segregation of rare earth dopants due to lower sintering temperature than crystals, to find strong mechanical properties with small grains at a low cost [12,13]. Commercial Lu 2 O 3 (Shin-Etsu Rare Earth, Tokyo, Japan; 99.99% purity), Nd 2 O 3 (Wako Pure Chemical Co. Inc., Tokyo, Japan; 99.9% purity) and LiF (Wako Pure Chemical Co. Inc., Tokyo, Japan; 99.9% purity) powders were used as the starting materials.…”
Section: Sps Procedures At the Tohoku Universitymentioning
confidence: 99%
“…At first, we have chosen to synthesize Nd 3+ -doped Lu 2 O 3 transparent ceramics by the Spark Plasma Sintering (SPS) method, a new and non-conventional one [12][13][14] as compared with conventional vacuum sintering or hot pressing methods. This new technique is comparatively simple and consumes less time than other conventional sintering methods.…”
Section: Introductionmentioning
confidence: 99%
“…When using intermediate pressures and standard graphite tools, a two-step pressure schedule might be advantageous to homogenize the microstructure. [144,150] However, possible contamination by carbon at least at the contact surface with graphite parts [151] and the creation of light-absorbing oxygen vacancies due to reducing conditions [152] both lower the in-line transmission. Usually, a postsintering annealing step in air improves the transparency.…”
Section: Transparent Ceramicsmentioning
confidence: 99%
“…Pure Lu 2 Ti 2 O 7 phase is virtually impossible at a temperature o1000 1C [11]. In our studies, the calcinations temperature is only 1000 1C.…”
Section: Synthesis Of the Lu 2 Ti 2 O 7 Nano-wiresmentioning
confidence: 99%