Effects of Some Parameters on Particle Size Distribution of Chitosan Nanoparticles Prepared by Ionic Gelation Method

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

13
60
0

Year Published

2015
2015
2023
2023

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 138 publications
(73 citation statements)
references
References 30 publications
13
60
0
Order By: Relevance
“…In both of them the band at 3436 cm -1 was assigned to NH 2 and OH stretching vibrations. The bands at 1657 cm -1 , 1598 cm -1 and 1320 cm -1 were attributed to Amide I, -NH 2 bending and Amide III, respectively (Vaezifar et al, 2013;Zhang et al, 2012). The only difference was observed at 1155 cm -1 in chitosan nanoparticles.…”
Section: Analysis Of Ft-ir Spectramentioning
confidence: 88%
See 1 more Smart Citation
“…In both of them the band at 3436 cm -1 was assigned to NH 2 and OH stretching vibrations. The bands at 1657 cm -1 , 1598 cm -1 and 1320 cm -1 were attributed to Amide I, -NH 2 bending and Amide III, respectively (Vaezifar et al, 2013;Zhang et al, 2012). The only difference was observed at 1155 cm -1 in chitosan nanoparticles.…”
Section: Analysis Of Ft-ir Spectramentioning
confidence: 88%
“…Preparation of chitosan nanoparticles was performed according to the procedure of Vaezifar et al (2013). Chitosan powder (5 mg) was dissolved in 1.0% (w/v) acetic acid.…”
Section: Preparation Of Chitosan Nanoparticlesmentioning
confidence: 99%
“…Pentasodium tripolyphosphate (TPP) anions were used to prepare chitosan nanoparticles according to the ionotropic gelation of chitosan . Chitosan powder (Sigma‐Aldrich) was dissolved in 1% acetic acid aqueous solutions.…”
Section: Methodsmentioning
confidence: 99%
“…The decreasing of crystallinity could be due to that chitosan nanoparticles are composed of a dense network structure of interpenetrating counter ions TPP, where the polymer chains crosslink with each other by TPP. Thus the XRD pattern of chitosan nanoparticles is characteristic of an amorphous polymer [20]. The surface and stability of the prepared chitosan nanoparticles was characterized using zeta potential, it was found that the surface was shown to be positively charged (+38 mv).…”
Section: Removal Of Fe (Ii) and Mn (Ii) From Wastewater …mentioning
confidence: 99%
“…Chitosan nanoparticles were formed spontaneously upon addition of 3 ml chitosan solution under vigorous magnetic stirring to 1 ml of an aqueous TPP solution (0.25% w/v), with a ratio of chitosan to TPP 3:1 at room temperature. Nanoparticles were separated by centrifugation at 9000×g for 20 min [20]. Chitosan nanoparticles were extensively rinsed with DI to remove any NaOH residues and dried at 40C o for 24 h before further use or analysis [21].…”
Section: Preparation Of Chitosan Nanoparticlesmentioning
confidence: 99%