2013
DOI: 10.1039/c3tc30378k
|View full text |Cite
|
Sign up to set email alerts
|

Efficient electrochromic performance of nanoparticulate WO3 thin films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

2
71
0

Year Published

2015
2015
2022
2022

Publication Types

Select...
7
2

Relationship

0
9

Authors

Journals

citations
Cited by 124 publications
(74 citation statements)
references
References 35 publications
(21 reference statements)
2
71
0
Order By: Relevance
“…For the entire scan rates, when the potential is swept from +1.5 V to -1.0 V a high cathodic current density with deep blue coloration is observed. This persistent increase in the cathodic current density specifies the reduction of W 6+ ionic state to the W 5+ state due to the intercalation of H + ions towards extreme cathodic potentials as a result of inter-valence charge transfer reactions which eventually causes the blue coloration [20]. This high negative current density observed approximately at the extreme negative potential scan is considered as the cathodic peak (spike) current density as reported in the literatures for WO 3 thin films [55,61].…”
Section: Cyclic Voltammetrymentioning
confidence: 92%
See 1 more Smart Citation
“…For the entire scan rates, when the potential is swept from +1.5 V to -1.0 V a high cathodic current density with deep blue coloration is observed. This persistent increase in the cathodic current density specifies the reduction of W 6+ ionic state to the W 5+ state due to the intercalation of H + ions towards extreme cathodic potentials as a result of inter-valence charge transfer reactions which eventually causes the blue coloration [20]. This high negative current density observed approximately at the extreme negative potential scan is considered as the cathodic peak (spike) current density as reported in the literatures for WO 3 thin films [55,61].…”
Section: Cyclic Voltammetrymentioning
confidence: 92%
“…When the film is deposited at RT, the collision relaxation period may not be long enough for the atoms to arrive to the ordered phase as the atoms do not gain enough kinetic energy from atomic collisions. It is proclaimed that such amorphous nature would favour electrochromic ion intercalation / deintercalation process [19,20]. The surface morphology of pure and V 2 O 5 doped thin films deposited at 100 W RF power were examined with field emission scanning electron microscope (FESEM).…”
Section: Structural and Morphological Studiesmentioning
confidence: 99%
“…The coloration efficiency (CE) was obtained from the spectra shown in Fig. 5a using the formula: CE = OD/Q mentioned by Dalavi et al [10]. These results are shown in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…The broad-angle XRD pattern of the resulted samples (Fig. 2d) exhibits a broad hump in the low 2θ region, which shows the amorphous nature of the material [33]. (Fig.…”
Section: Preparation Of Mscssmentioning
confidence: 96%