Carbofuran photodegradation in water using zinc oxide nanoparticles as a catalyst was examined as well as some parameters influencing its percentage degradation rate such as zinc oxide load, initial concentration of carbofuran, the temperature of the reaction, the initial pH of the solution, and doping of zinc oxide nanoparticles with 5% (w:w) silver. Zinc oxide and Ag-doped zinc oxide nanoparticles were produced using solvothermal and photoreduction methods, respectively, and silver doping effects on the structural, optical, and photocatalytic properties of zinc oxide nanoparticles were investigated using XRD, UV-VIS spectrophotometer, TEM, SEM, SEM/EDX, and FTIR. The average diameter of the synthesized samples was 26.6, 30.55 nm for undoped zinc oxide and Ag-doped zinc oxide, respectively. Zinc oxide doping with silver did not change the shape of the zinc oxide crystal, but decreased the reflection in the visible region, as well as the energy of the bandgap, and increased the zinc oxide photocatalytic activity.