“…Meanwhile, the average surface roughness for BGST thin films were 0.632, 0.564, and 0.487 nm at annealing temperature of 200, 240, and 280°C, respectively, whereas the grain sizes (mean diameter) were 238.4, 219.0, and 185.1 nm, respectively. The average surface roughness for BTST thin films were 1.087, 0.4870, and 0.2317 nm at temperature 200, 240, 280°C, respectively, whereas the grain size (mean diameter) are 158.7, 291.1, and 396.7 nm, respectively [9]. Thus, we found that addition of dopants significantly alters the surface roughness and grain size, and a similar feature is expected for rare-earth, e.g., lanthanum oxide (La 2 O 3 ) dopant on thin films.…”