Enhancing piezoelectric properties of bacterial cellulose films by incorporation of MnFe2O4 nanoparticles

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2

Citation Types

0
23
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 48 publications
(23 citation statements)
references
References 49 publications
0
23
0
Order By: Relevance
“…In the bending mode, the BC films showed higher piezoelectric responses with values ranging from 55-158 pC/N and 40-71 pC/N for BC-glucose and BC-crude glycerol films, respectively. The bending mode piezoelectric sensitivities from BC-glucose is higher to that observed in our previous study using BC-glucose films synthesized by K. xylinus DSM 2325 (Sriplai et al 2020). This implies the application potential of K. rhaeticus ENS9a BC films in sensing applications, for instance in energy harvesting applications where bending mode sensitivities are critical.…”
Section: Piezoelectric Sensitivities Of Bc Filmsmentioning
confidence: 52%
See 1 more Smart Citation
“…In the bending mode, the BC films showed higher piezoelectric responses with values ranging from 55-158 pC/N and 40-71 pC/N for BC-glucose and BC-crude glycerol films, respectively. The bending mode piezoelectric sensitivities from BC-glucose is higher to that observed in our previous study using BC-glucose films synthesized by K. xylinus DSM 2325 (Sriplai et al 2020). This implies the application potential of K. rhaeticus ENS9a BC films in sensing applications, for instance in energy harvesting applications where bending mode sensitivities are critical.…”
Section: Piezoelectric Sensitivities Of Bc Filmsmentioning
confidence: 52%
“…Oven-dried BC films prepared from MA/9 medium containing 2% glucose and crude glycerol were used in this study (see section BC film preparation and dry weight measurements). Sensor construction, piezoelectric sensitivity measurement setup and sensitivity calculations were conducted as described previously (Mangayil et al 2017;Sriplai et al 2020) with slight variations. The hydrated BC film was sandwiched between two silver electrodes (100 nm) vacuum evaporated on poly(ethylene-terephthalate) (PET) film and left to dry O/N at 45°C resulting in a self-adhered construct.…”
Section: Piezoelectric Sensitivity Measurementsmentioning
confidence: 99%
“…8B). As demonstrated in the four FTIR spectra, the wide peak around 3352 cm −1 is assigned to the O-H stretching, while the peak around 2900 cm −1 is related to C-H stretching 53 . The water bending vibrations peaked at 1639 cm −1 , while the peaks around 1357 cm −1 indicate the C-H bending.…”
mentioning
confidence: 79%
“…In order to overcome such limitations, synthetic and biodegradable polymers, as well as polymeric composites have been used to develop PENGs (Sun, Zeng, & Li, 2020). For instance, polysaccharides, such as chitosan (Hänninen, Rajala, Salpavaara, Kellomäki, & Tuukkanen, 2016, cellulose (Rajala et al, 2016;Sriplai et al, 2020;Tuukkanen & Rajala, 2018) and bacterial cellulose (Mangayil et al, 2017) have been reported to be used as lightweight and flexible piezoelectric materials. However, PENGs are known to be efficient when the frequency of the mechanical excitation ranges 60−100 Hz (Han et al, 2013;Liu, Zhong, Lee, Lee, & Lin, 2018).…”
Section: Introductionmentioning
confidence: 99%