Examination of the effect of Sc on 2000 and 7000 series aluminium alloy castings: for improvements in fusion welding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

1
57
0

Year Published

2006
2006
2023
2023

Publication Types

Select...
5
4

Relationship

0
9

Authors

Journals

citations
Cited by 108 publications
(62 citation statements)
references
References 9 publications
1
57
0
Order By: Relevance
“…Experiments simulating weld bead solidification by wedge-shaped casting of scandium-containing AA 2024 and AA 7475 aerospace alloys also confirm the positive effects of scandium on the microstructure. [67] B. Welding Process…”
Section: A Materialsmentioning
confidence: 99%
“…Experiments simulating weld bead solidification by wedge-shaped casting of scandium-containing AA 2024 and AA 7475 aerospace alloys also confirm the positive effects of scandium on the microstructure. [67] B. Welding Process…”
Section: A Materialsmentioning
confidence: 99%
“…Thus, a typical heat treatment for 6013 alloy is a T6, at 180-190 °C for a few hours. In 7475 alloy the typical precipitates are MgZn 2 (η or η') and CuMgAl 2 S phase (Norman et al, 2003). The mechanical data of 7475 alloy were given in the T761 state since it is one of the most common state for this alloy.…”
Section: B Analysis Of the Behaviour Of The Base Alloysmentioning
confidence: 99%
“…2(e)] a fine cast grain structure can be observed. According to the literature [23] this is due to the finely distributed Al 3 Sc x Zr 1 À x dispersoids, which can act as inhomogeneous nucleation sites for grain nucleation.…”
Section: Experimental Workmentioning
confidence: 99%