Fabricación de filamentos de PCL y PVA reforzados con HAp para ser usados en impresión 3D

Abstract: El objetivo principal de este trabajo fue la fabricación de filamentos de alcohol polivinílico (PVA) y policaprolactona (PCL) para ser usados en impresión 3D con tecnología de modelado por deposición fundida de filamentos (FDM). El estudio se orientó primeramente en fabricar los filamentos de estos biopolímeros por extrusión y posteriormente estos se reforzaron internamente con hidroxiapatita (HAp) para así mejorar sus propiedades mecánicas. Previo al proceso de manufactura, el PVA, PCL y HAp se caracterizaron… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

1
2
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(3 citation statements)
references
References 19 publications
1
2
0
Order By: Relevance
“…The X‐ray diffractograms in Figure 7 allow us to evaluate the crystallinity of the films where amorphous and C crystalline zones in monolayer films, except for PLA films, show broad zones characteristic of amorphous polymers. The polymer with the highest crystallinity is PCL, with 25.45% and crystalline peaks of great intensity ty and very well defined at 21.66° and 24.1° at 2θ, values like those obtained by Guillén‐Girón (2018).…”
Section: Resultssupporting
confidence: 66%
“…The X‐ray diffractograms in Figure 7 allow us to evaluate the crystallinity of the films where amorphous and C crystalline zones in monolayer films, except for PLA films, show broad zones characteristic of amorphous polymers. The polymer with the highest crystallinity is PCL, with 25.45% and crystalline peaks of great intensity ty and very well defined at 21.66° and 24.1° at 2θ, values like those obtained by Guillén‐Girón (2018).…”
Section: Resultssupporting
confidence: 66%
“…The infrared spectra corresponding to the PCL-based materials are shown in Figure , in this case normalized to the carbonyl stretching band at 1721 cm –1 . The asymmetric and symmetric C–H stretching vibrations of the methylene groups appear at 2942 and 2865 cm –1 , respectively, , together with the asymmetric and symmetric stretching of the C–O–C group, at 1242 and 1167 cm –1 , respectively. , …”
Section: Resultsmentioning
confidence: 98%
“…Regarding the presence of solvents in the blow spun PEO, neither the characteristic band at 665 The infrared spectra corresponding to the PCL-based materials are shown in Figure 3, in this case normalized to the carbonyl stretching band at 1721 cm −1 . The asymmetric and symmetric C−H stretching vibrations of the methylene groups appear at 2942 and 2865 cm −1 , respectively, 43,44 together with the asymmetric and symmetric stretching of the C−O−C group, at 1242 and 1167 cm −1 , respectively. 44,45 As in the case of PEO, the lack of significant changes in the position or relative intensities of the bands indicates that the rotational speed of the collector does not modify the conformation of the PCL chains and that the chloroform is fully evaporated during the formation of the fibers in the SBS process.…”
Section: Resultsmentioning
confidence: 99%