2018
DOI: 10.1039/c8ra07260d
|View full text |Cite
|
Sign up to set email alerts
|

Influence of citrate on phase transformation and photoluminescence properties in LaPO4 and LaPO4:Eu

Abstract: The hexagonal and monoclinic phase LaPO4:Eu nanostructures have been controllably synthesized using a citrate-induced hydrothermal process at 100 °C.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 8 publications
(3 citation statements)
references
References 35 publications
0
3
0
Order By: Relevance
“…These measurements were performed using JCPDS no. 01-083-0651 [23]. The absence of impurities is indicated by the observation of diffraction peaks, which show that no additional peaks are present and that the peaks are sharply defined.…”
Section: Xrd Analysismentioning
confidence: 96%
“…These measurements were performed using JCPDS no. 01-083-0651 [23]. The absence of impurities is indicated by the observation of diffraction peaks, which show that no additional peaks are present and that the peaks are sharply defined.…”
Section: Xrd Analysismentioning
confidence: 96%
“…The XRD spectra of LaPO 4 NRs, LaPO 4 NPs, La 2 S 3 NPs, and La 2 O 3 NPs show characteristic peaks of LaPO 4 , LaPO 4 , La 2 S 3 , and La 2 O 3 . 29,40 The La ion release ability of the four La based NMs in water followed the order of La 2 S 3 NPs > La 2 O 3 NPs > LaPO 4 NRs ≈ LaPO 4 NPs (Fig. S1A †).…”
Section: Characterization Of Different La Based Nmsmentioning
confidence: 99%
“…CPOT was synthesized by the solvothermal method. 36,37 Firstly, 25 mL of CeNO 3 solution (0.2 M), 25 mL of TbNO 3 solution (0.2 M), and 50 mL of citric acid solution (0.2 M) were prepared. Subsequently, CeNO 3 and TbNO 3 pre-formulations were added to 30 mL of ethylene glycol (the specific ratio of Ce 3+ and Tb 3+ was adjusted according to specific needs, and the total amount was 0.15 mmol), and then 750 μL of citric acid (2 M) pre-formulation was injected to form a complex of lanthanide and citric acid.…”
Section: Preparation Of Cpot Nanospheresmentioning
confidence: 99%