Influence of Enamel Conditioning on the Shear Bond Strength of Different Adhesives

Abstract: The highest shear forces were found for the conventional composites Transbond™ XT and Cool- Bond™ in combination with conventional etching. Air abrasion alone and in combination with phosphoric acid etching showed no advantages compared with phosphoric acid etching alone and, therefore, cannot be recommended.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
22
1
9

Year Published

2015
2015
2022
2022

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 17 publications
(33 citation statements)
references
References 33 publications
1
22
1
9
Order By: Relevance
“…Atualmente, o procedimento mais tradicional é o condicionamento com ácido fosfórico (Waveren Hogervorst et al, 2000;Canay et al, 2000;Medhi et al, 2009;Brauchli et al, 2010;Türköz;Ulusoy, 2012); entretanto, com o propósito de obter melhores forças adesivas preservando a integridade do esmalte, outros métodos de condicionamento têm sido propostos, como diferentes ácidos (ácido sulfúrico diluído, ácido maleico e ácido poliacrílico) (Ärtun;Bergland, 1984;Olsen et al, 1997b;Bishara et al, 2000), laser de alta potência (Berk et al, 2008;Türköz;Ulusoy, 2012), self etching primers (Halpern;Rouleau, 2010;Türköz;Ulusoy, 2012) e jato de óxido de alumínio (Olsen et al, 1997a;Reisner et al, 1997;Canay et al, 2000;Berk et al, 2008;Medhi et al, 2009;Brauchli et al, 2010;Halpern;Rouleau, 2010, Cal-Neto et al, 2011Suma et al, 2012;Türköz;Ulusoy, 2012).…”
Section: Lista De Figurasunclassified
See 4 more Smart Citations
“…Atualmente, o procedimento mais tradicional é o condicionamento com ácido fosfórico (Waveren Hogervorst et al, 2000;Canay et al, 2000;Medhi et al, 2009;Brauchli et al, 2010;Türköz;Ulusoy, 2012); entretanto, com o propósito de obter melhores forças adesivas preservando a integridade do esmalte, outros métodos de condicionamento têm sido propostos, como diferentes ácidos (ácido sulfúrico diluído, ácido maleico e ácido poliacrílico) (Ärtun;Bergland, 1984;Olsen et al, 1997b;Bishara et al, 2000), laser de alta potência (Berk et al, 2008;Türköz;Ulusoy, 2012), self etching primers (Halpern;Rouleau, 2010;Türköz;Ulusoy, 2012) e jato de óxido de alumínio (Olsen et al, 1997a;Reisner et al, 1997;Canay et al, 2000;Berk et al, 2008;Medhi et al, 2009;Brauchli et al, 2010;Halpern;Rouleau, 2010, Cal-Neto et al, 2011Suma et al, 2012;Türköz;Ulusoy, 2012).…”
Section: Lista De Figurasunclassified
“…Desta forma, devido ao fato dos estudos que avaliaram o condicionamento do esmalte com óxido de alumínio associado ao ácido fosfórico na resistência à colagem (Canay et al, 2000;Wiechmann, 2000;Brosh et al, 2005;Miles, 2008;Brauchli et al, 2010;Cal-Neto et al, 2011;Pakshir et al, 2012;Suma et al, 2012;Türköz;Ulusoy, 2012) mostrarem resultados variados e verificando-se que esta metodologia é utilizada por alguns clínicos para aumentar a adesão dos braquetes nas faces linguais (Fillion, 1999;Wiechmann et al, 2000;Miles, 2008) O condicionamento do esmalte é um passo essencial antes da colagem dos braquetes. Durante esta etapa a película aderida ao dente é removida e rugosidades são criadas na superfície do esmalte, o que são necessárias para uma boa fixação do agente de colagem (Medhi et al, 2009).…”
Section: Lista De Figurasunclassified
See 3 more Smart Citations