Investigation on the passivated Si/Al2O3 interface fabricated by non-vacuum spatial atomic layer deposition system

Abstract: . Investigation on the passivated Si/Al2O3 interface fabricated by non-vacuum spatial atomic layer deposition system, nano Online (2016). DOI: https://doi.org/10.1515/nano.11671_2015.154Originally published in: Shui-Yang Lien, Chih-Hsiang Yang, Kuei-Ching Wu, Chung-Yuan Kung. Investigation on the passivated Si/Al2O3 interface fabricated by nonvacuum spatial atomic layer deposition system, Nanoscale Research Letters. 10 (2015). DOI: https://doi.org/10.1186/s11671-015-0803-9Lien et al., 2015. This is an Open Acc… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2019
2019
2019
2019

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(5 citation statements)
references
References 21 publications
0
5
0
Order By: Relevance
“…Afterwards, rear‐side emitter removal process was performed, and the surfaces were cleaned by hot HNO 3 solution followed by HF‐Dip and DI water rinsing. For iV oc samples and PERC solar cells, a 6‐nm‐thick Al 2 O 3 layer was then deposited on the rear‐side by using ultrafast spatial ALD process . This step was followed by the so‐called outgassing process, which is a 10‐minute low temperature annealing under N 2 at 550°C performed mainly to avoid blistering of the rear‐side stack layer .…”
Section: Methodsmentioning
confidence: 99%
See 3 more Smart Citations
“…Afterwards, rear‐side emitter removal process was performed, and the surfaces were cleaned by hot HNO 3 solution followed by HF‐Dip and DI water rinsing. For iV oc samples and PERC solar cells, a 6‐nm‐thick Al 2 O 3 layer was then deposited on the rear‐side by using ultrafast spatial ALD process . This step was followed by the so‐called outgassing process, which is a 10‐minute low temperature annealing under N 2 at 550°C performed mainly to avoid blistering of the rear‐side stack layer .…”
Section: Methodsmentioning
confidence: 99%
“…However, a high positive Q f present in the SiN x layer is found to be detrimental for the passivation of boron highly doped p + emitters on n‐type solar cell architectures or back surface field (BSF) present in p‐PERC or p‐PERT solar cell architectures, as it induces a depletion layer near the surface which increases the charge carrier recombination rate . Thus, the surface passivation of such p + emitter/BSF is generally realized by applying either ultrathin (<10 nm) silicon oxide (SiO x ) or aluminum oxide (AlO x ) layers, which are usually capped by a thicker protective SiN x film (70‐150 nm) . Particularly, AlO x /SiN x stacks lead to very low SRV (≤10 cm.s −1 ) on moderately doped n‐type and p‐type Si wafers and correspondingly low j 0e (≤ 50 fA.cm −2 ) on p + emitter/BSF .…”
Section: Introductionmentioning
confidence: 99%
See 2 more Smart Citations
“…Since some carriers recombine in the bulk and some recombine near the surface, carrier lifetimes could be improved after AlO x passivation owing to the reduction of surface recombination velocity or, in other words, the reduction of recombination rate of carriers on the surface of the wafers. Therefore, lifetime improvements were mainly attributed to the effect of AlO x passivation and can be explained by the elimination of the recombination centers including defects and dangling bonds at or near the surface owing to the formation of interfacial SiO x [22,23]. The increase of SiO x at the interface increases the passivation quality and can reduce dangling bonds by bonding of the oxygen atoms of SiO x with negatively charged Al atoms [24].…”
Section: Resultsmentioning
confidence: 99%