Mechanical and electrical properties of In-Bi solder at Bi2212 superconductor interface with annealed Ag spray layers and Ag precoating layers

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2

Citation Types

0
2
0

Year Published

2015
2015
2015
2015

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(2 citation statements)
references
References 15 publications
0
2
0
Order By: Relevance
“…Solder points have also been used between bulk Bi-2212 current leads, but problems have been found with the wetting of the ceramic surface with solders. Applying a metallic layer between the solder and the ceramic improves the wettability of the solder and thus increases the joint strength [103]. An example of this is In-Bi solders for joining Bi-2212 superconducting tubes by pre-coating Ag layers on the Bi-2212 surface [103].…”
Section: Bi-2212 Tapementioning
confidence: 99%
See 1 more Smart Citation
“…Solder points have also been used between bulk Bi-2212 current leads, but problems have been found with the wetting of the ceramic surface with solders. Applying a metallic layer between the solder and the ceramic improves the wettability of the solder and thus increases the joint strength [103]. An example of this is In-Bi solders for joining Bi-2212 superconducting tubes by pre-coating Ag layers on the Bi-2212 surface [103].…”
Section: Bi-2212 Tapementioning
confidence: 99%
“…Applying a metallic layer between the solder and the ceramic improves the wettability of the solder and thus increases the joint strength [103]. An example of this is In-Bi solders for joining Bi-2212 superconducting tubes by pre-coating Ag layers on the Bi-2212 surface [103].…”
Section: Bi-2212 Tapementioning
confidence: 99%