Microstructure and mechanical properties of nano-Y2O3dispersed ferritic steel synthesized by mechanical alloying and consolidated by pulse plasma sintering

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
9
0

Year Published

2013
2013
2020
2020

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 37 publications
(9 citation statements)
references
References 38 publications
0
9
0
Order By: Relevance
“…Composite selected for investigation contains 95 wt% Fe and 5 wt% Al 2 O 3 . Mixed powder was dry ball milled with the powder to ball ratio of 1:2 using zirconia balls as the grinding and mixing media (Karak et al 2012). Initially the powder of electrolytic iron (Fe) and aluminum oxide (Al 2 O 3 ) was milled in the ball mill for a period of 1 h. Thereafter, 1% glycerine and 1% dextrin were added to the above mixture and the whole mixture was milled for a period of 1 h again.…”
Section: Preparationmentioning
confidence: 99%
“…Composite selected for investigation contains 95 wt% Fe and 5 wt% Al 2 O 3 . Mixed powder was dry ball milled with the powder to ball ratio of 1:2 using zirconia balls as the grinding and mixing media (Karak et al 2012). Initially the powder of electrolytic iron (Fe) and aluminum oxide (Al 2 O 3 ) was milled in the ball mill for a period of 1 h. Thereafter, 1% glycerine and 1% dextrin were added to the above mixture and the whole mixture was milled for a period of 1 h again.…”
Section: Preparationmentioning
confidence: 99%
“…Karak et al [19] reported that ferritic ODS steel with compositions of Fe-13.5Cr-2.0Al-0.5Ti + 1.0Y 2 O 3 , Fe-17.5Cr-2.0Al-0.5Ti + 1.0Y 2 O 3 , Fe-21.5Cr-2.0Al-0.5Ti + 1.0Y 2 O 3 and Fe-25.5Cr-2.0Al-0.5Ti + 1.0Y 2 O 3 produced by MA and SPS exhibited 1.5-2 times greater compressive strength and improved ductility than those produced by hot press sintering and HIP, which was ascribed to the presence of 10-20 nm Y 2 Ti 2 O 7 or Y 2 O 3 nano-particles observed by TEM. Sun [20,21], Xia [22] and Gao et al [23] fabricated Fe-14Cr-…”
Section: Introductionmentioning
confidence: 98%
“…However, all the three alloys show better compressive strength than the 17.5Cr ferritic ODS steel (79.0 Fe-17.5Cr-2.0Al-0.5Ti) fabricated via pulse plasma sintering and high pressure sintering by Karak et al [38]. The improvement in the compressive strength observed in the present alloys compared to the alloys developed by Karak et al [43] may be corroborated to the presence of nano complex oxides that can arrest the dislocation motion along the grain boundary during deformation.…”
Section: Hardness Of the Consolidated Ods Specimensmentioning
confidence: 48%