DOI: 10.1007/s12598-015-0492-7
|View full text |Cite
|
Sign up to set email alerts
|

Microstructure and wear-resistant properties of NiCr–Cr3C2 coating with Ni45 transition layer produced by laser cladding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
6
0

Year Published

2016
2016
2024
2024

Publication Types

Select...
8
1
1

Relationship

0
10

Authors

Journals

citations
Cited by 24 publications
(6 citation statements)
references
References 9 publications
0
6
0
Order By: Relevance
“…The carbides of Cr were commonly found in the HEA containing both Cr and C. 37,38 Previous studies have reported that the mechanical and tribological properties were improved with the addition of Cr 3 C 2 . 39,40 The carbides of Cr have been verified with high hardness, strength and excellent thermal stability, which could impede the dislocation motion and strengthen the composite significantly. 40 Thus, the outstanding tribological properties of the HEA/0.6 wt% GO composite were also attributed to the strengthening effect of the carbide of Cr in this study.…”
Section: Resultsmentioning
confidence: 99%
“…The carbides of Cr were commonly found in the HEA containing both Cr and C. 37,38 Previous studies have reported that the mechanical and tribological properties were improved with the addition of Cr 3 C 2 . 39,40 The carbides of Cr have been verified with high hardness, strength and excellent thermal stability, which could impede the dislocation motion and strengthen the composite significantly. 40 Thus, the outstanding tribological properties of the HEA/0.6 wt% GO composite were also attributed to the strengthening effect of the carbide of Cr in this study.…”
Section: Resultsmentioning
confidence: 99%
“…Thus Ag will not react with other elements and remain as Ag in composites. Because of the rapid sintering of SPS technique, the Cr 3 C 2 decarburizes forming Cr 7 C 3 [23]. Compared to Cr 3 C 2 , Cr 7 C 3 has higher thermal stability, strength and wear resistance, which can improve the strength of composites.…”
Section: Resultsmentioning
confidence: 99%
“…NiCr-Cr3C2 composites ceramic coatings are widely used for surface strengthening of components due to high temperature resistance, wear resistance and corrosion resistance (12,13) . Huang et al reported that the Ni based composite coatings have been obtained by using the plasma spray welding process and mixed powders (NiCrBSi + NiCr-Cr3C2 + WC)., exhibited enhance the coating hardness and good mechanical properties (14) .…”
Section: Farvizi Et Al Added a Low Weight Percentage Of Hard Al2o3mentioning
confidence: 99%