“…The morphology of the drawn nanocomposite fibers (DR = 8) was also examined using the SEM method. It is well known [ 3 , 32 , 33 , 34 , 35 , 36 , 37 , 38 ] that during high-temperature orientational drawing, the lamellae morphology transforms in the fibrillar one. As an example, the SEM micrograph of the internal structure of the fiber with the added nanodiscs is presented in Figure 6 .…”