“…The reasoning extends then to Q 2 , Q 3 , and Q 4 meaning two, three, and four sharing oxygen atoms, respectively. Upon contacting glass or a silica-rich mineral with an alkaline environment it is expected that the amount of Q 0 -Q 3 species increase with time due to silica depolymerization, a phenomenon that can be tracked since each Q n species appear at distinct frequencies in the Raman spectrum [7][8][9] .Zinc (Zn 2+ ) species, as a retarder, have been under study where its mechanistic and kinetic aspects have been taken into consideration [10][11][12][13] . Zinc oxide (ZnO), for instance, is thought to dissolve into Zn 2+ which prolongs the setting time by sequestering calcium ions (Ca 2+ ) and forming calcium zincate [Ca(Zn(OH) 3 ) 2 .2H 2 O] 11 .…”