2012
DOI: 10.1039/c2cy20325a
|View full text |Cite
|
Sign up to set email alerts
|

Nanoconfinement of Ni clusters towards a high sintering resistance of steam methane reforming catalysts

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
20
0

Year Published

2015
2015
2023
2023

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 20 publications
(21 citation statements)
references
References 36 publications
1
20
0
Order By: Relevance
“…4a the prole of the Ni8 sample was shown as an example). A similar behavior was previously observed by Li and coworkers 50 and by Guil-López and coworkers, 51 15 and/or small sizes of NiO would be conducive to this process, since there are more atoms at the interface promoting the solid-solid reaction. 52 To study the role of the amount of Ni and the oxide matrix on the reduction/oxidation behavior, TPR/TPO/TPR proles of high-loaded Ni/Al catalysts obtained from silicates and carbonates (Ni68 and Ni68-CO 3 ), previously characterized by XRD, were investigated (Fig.…”
Section: Ni Speciation In Catalystssupporting
confidence: 85%
“…4a the prole of the Ni8 sample was shown as an example). A similar behavior was previously observed by Li and coworkers 50 and by Guil-López and coworkers, 51 15 and/or small sizes of NiO would be conducive to this process, since there are more atoms at the interface promoting the solid-solid reaction. 52 To study the role of the amount of Ni and the oxide matrix on the reduction/oxidation behavior, TPR/TPO/TPR proles of high-loaded Ni/Al catalysts obtained from silicates and carbonates (Ni68 and Ni68-CO 3 ), previously characterized by XRD, were investigated (Fig.…”
Section: Ni Speciation In Catalystssupporting
confidence: 85%
“…It is clear that after calcination the structure of the Ni‐HT catalyst shows a layered ribbon structure . Moreover, the STEM image reveals a highly porous catalyst material and it seems that the porosity has an ordered structure.…”
Section: Resultsmentioning
confidence: 70%
“…Moreover, the STEM image reveals a highly porous catalyst material and it seems that the porosity has an ordered structure. The dual pore size distribution with average pore size about 3.5 and 18 nm was confirmed by detailed TEM analysis and N 2 physisorption . In an earlier publication, tomographic reconstruction showed that the pores have a rectangular morphology and regular distribution within the plates …”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…Nanoconfinement of Ni particles by self-assembly of Ni atoms inside the nanoribbons of hydrotalcite-derived mixed oxide provided increased catalytic stability for methane steam reforming, compared to Ni supported on commercial support surface. [59] Metal embedment has also proven to be an efficient stabilization method for lactic acid production from glycerol. Morales et al showed that MFI constituted a stabilizing matrix for Sn and significantly decreased leaching of said Sn while slowing down deactivation in comparison to bifunctional carbon-silica composites and BEA zeolites.…”
Section: Irreversible Deactivation Via Sintering And/or Leaching Of Smentioning