“…However, the sintered ceramics prepared from different batches show different dilatometry results, and further research is under way. Such a strong NTE exceeds most of those of the NTE framework structure oxides, including NbVO 5 ( α v ∼ −6.63 × 10 –6 K –1 , 298–873 K), NbPO 5 ( α v ∼ −11 × 10 –6 K –1 , 673–973 K), α -Cu 2 V 2 O 7 ( α v ∼ −9.29 × 10 –6 K –1 , 100–573 K), , ThP 2 O 7 ( α v ∼ −10.5 × 10 –6 K –1 , 473–1174 K), Y 2 W 3 O 12 ( α v ∼ −20.9 × 10 –6 K –1 , 15–1373 K), and Sc 2 W 3 O 12 ( α v ∼ −6.67 × 10 –6 K –1 , 10–1200 K), and is even stronger than the average α v of ZrW 2 O 8 from 0.3 to 1050 K ( α v ∼ −21.9 × 10 –6 K –1 , 0.3–1050 K) . In 2019, Goodwin et al proposed the metrics of “NTE capacity”, denoted by χ α , to unbiasedly compare the NTE properties in different systems.…”