Optical band gap and photoluminescence studies of Eu3+-doped zinc silicate derived from waste rice husks

Abstract: In this study, investigation on photoluminescence and optical properties of europium doped zinc silicate (Zn2SiO4:Eu3+) glass ceramics derived from white rice husk ash as potential silica source have been done. Undoped and 3 wt. % of europium doped zinc silicate were prepared by solid state method and sintered at 600-1000 °C for 2 h. XRD analysis revealed the phase formation of amorphous, α or β-Zn2SiO4:Eu3+ phases of the glass and glass ceramic samples. FESEM results show the samples were irregular in shapes … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
22
0
1

Year Published

2020
2020
2024
2024

Publication Types

Select...
10

Relationship

5
5

Authors

Journals

citations
Cited by 45 publications
(24 citation statements)
references
References 41 publications
1
22
0
1
Order By: Relevance
“…In order to determine the size of the crystal, the type of crystal, and the surface morphology of the zinc silicate glass and glass-ceramics samples, the FESEM analysis was done. From our observations, at the lower temperatures of 27 • C and 700 • C there were no grain growth, showing a clear glassy surface that tallies with the XRD result where at 27 • C and 700 • C the sample was still in an amorphous phase [16]. Meanwhile, as the sintering temperature increased to 750 • C and 800 • C, the microstructure of the sample still did not show a regular shape (irregular) and started to aggregate among each other.…”
Section: Discussionsupporting
confidence: 86%
“…In order to determine the size of the crystal, the type of crystal, and the surface morphology of the zinc silicate glass and glass-ceramics samples, the FESEM analysis was done. From our observations, at the lower temperatures of 27 • C and 700 • C there were no grain growth, showing a clear glassy surface that tallies with the XRD result where at 27 • C and 700 • C the sample was still in an amorphous phase [16]. Meanwhile, as the sintering temperature increased to 750 • C and 800 • C, the microstructure of the sample still did not show a regular shape (irregular) and started to aggregate among each other.…”
Section: Discussionsupporting
confidence: 86%
“…Por lo tanto, la E opt del sistema disminuye de 4,50 a 4,41 eV en orden creciente de ZnO y la disminución es causada por la naturaleza covalente del enlace Zn-O. Khaidir et al (2019) investigaron la fotoluminiscencia y propiedades ópticas de vidrios y vitrocerámicas de silicato de zinc dopado con europio (Zn2SiO 4:Eu 3+) derivado de cenizas de cáscara de arroz blanco como fuente potencial de sílice mediante el método de sinterización. El análisis difracción de rayos X (XRD) reveló la formación de fases amorfas, a o ß-Zn2SiO4: Eu3+ en las muestras de vidrio y vitrocerámica.…”
Section: Producción De Vitrocerámicas Basadas En Cenizasunclassified
“…Several past studies have proven that silica can be extracted from various agricultural wastes, such as rice husk, rice straw, sugarcane bagasse, corn cob and palm ash [8,[11][12][13][15][16][17][21][22][23][24][25][26][27][28]. However, information regarding its synthesis from coconut husk waste is limited.…”
Section: Introductionmentioning
confidence: 99%