Ordered Gold Nanostructure Assemblies Formed By Droplet Evaporation

Abstract: The order of gold: Ordered assemblies of gold nanostructures are produced by droplet evaporation from single‐ and two‐component systems. The ordering of the assemblies is highly dependent on the shape and size of gold nanostructures and includes nanorods, nanocubes, polyhedra, and bipyramids. The two‐photon‐excited luminescence of ordered gold nanorod assemblies is larger than that of disordered nanorod assemblies.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

5
183
0
1

Year Published

2010
2010
2022
2022

Publication Types

Select...
5
3

Relationship

1
7

Authors

Journals

citations
Cited by 260 publications
(189 citation statements)
references
References 52 publications
5
183
0
1
Order By: Relevance
“…Different geometries of gold nanoparticles were assembled by solvent drop evaporation using concentrated aqueous dispersions of particles ( Figure 3). [29] The particles were stabilized by A. Stein et al…”
Section: Long-range Self-assembly Of Nonspherical Particlesmentioning
confidence: 99%
“…Different geometries of gold nanoparticles were assembled by solvent drop evaporation using concentrated aqueous dispersions of particles ( Figure 3). [29] The particles were stabilized by A. Stein et al…”
Section: Long-range Self-assembly Of Nonspherical Particlesmentioning
confidence: 99%
“…The DEFA presented herein complements several assembly strategies that have been developed to create superlattices of anisotropic nanostructures including evaporationinduced [19,20] and sedimentation-based methods, [8] as well as ones based upon the manipulation of electrostatic, [21,22] entropic, [13,[23][24][25][26][27][28] block copolymer, [29,30] and biological recognition interactions. [31] However, unlike the majority of these methods, our approach yields reversible crystals with tunable lattice constants in situ.…”
mentioning
confidence: 99%
“…Synthesis of Au Nanocubes : Au nanocubes were prepared according to the previously reported procedure. [ 55 ] The seeds were prepared by the addition of a freshly prepared, ice-cold aqueous NaBH 4 solution (0.01 M , 0.6 mL) into an aqueous mixture solution composed of HAuCl 4 (0.01 M , 0.25 mL) and CTAB (0.1 M , 7.5 mL), followed by vigorously string for 2 min. The resulting seed solution was kept at room temperature for 1 h before use.…”
Section: Methodsmentioning
confidence: 99%
“…[ 1,2 ] These NP superlattices have shown a variety of applications in biosensing, [ 3 ] catalysis, [ 4 ] photonic crystals, [ 5 ] nanoelectronics, [ 6,7 ] and energy conversion and storage. [ 8 ] Typical strategies for the fabrication of superlattices include such as drying mediated method, [ 9 ] assembly under external fi eld (e.g., electric and magnetic fi elds), [ 10 ] and ligand directed assembly. [11][12][13][14] The spatial arrangement (i.e., symmetry, interparticle space, small 2016, 12, No.…”
Section: Introductionmentioning
confidence: 99%