Abstract:Copper Indium Selenide (CIS) thin films were pulse electrodeposited at room temperature and at different duty cycles in the range of 6 – 50 %. Deposition current density was kept constant at 5 ma cm-2 in the present work. The total deposition time was 60 min. The precursors used were AR grade 0.3 M of each CuCl2 and InCl3, along with 0.2 M of SeO2. Thickness of the films estimated by Mitutoyo surface profilometer varied in the range of 0.8 to 1.2 μm with increase of duty cycle. XRD patterns of CIS films deposi… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.