“…On top of the buffer layer, we deposited an 80 nm-thick a-Si film as an active layer at a sputtering condition of 4.0 W/cm 2 and , and thus, the layer stacking is inherently unstable [9]. Since the a-Si film is completely melted during the SLS process, it is very important to suppress liquid film dewetting during the solidification of Si.…”