“…1c) provided better depth resolution for the three layers, containing Ni, and also a sharper interface conductive layernon-conductive substrate. This lower pulse width has also allowed for a significant increase in the Nd sensitivity because spacecharge effects occurring at the instrument interface for long pulses [14] are not evident at short pulses. Therefore, considering signal intensities and depth resolution of the deposited layers on glass, 0.16 ms pulse width and 1.32 ms period were selected for subsequent experiments.…”