Porous magnesium/PLGA composite scaffolds for enhanced bone regeneration following tooth extraction

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

2
105
0
1

Year Published

2016
2016
2024
2024

Publication Types

Select...
6
2

Relationship

0
8

Authors

Journals

citations
Cited by 180 publications
(108 citation statements)
references
References 45 publications
2
105
0
1
Order By: Relevance
“…The total porosity, P total (the total pore volume divided by the volume of the scaffold), can be Where ρ s is the density of metallic Zn (7.14 g/cm 3 ).…”
Section: Morphology and Structural Characterization Of Porous Zn Scafmentioning
confidence: 99%
See 1 more Smart Citation
“…The total porosity, P total (the total pore volume divided by the volume of the scaffold), can be Where ρ s is the density of metallic Zn (7.14 g/cm 3 ).…”
Section: Morphology and Structural Characterization Of Porous Zn Scafmentioning
confidence: 99%
“…Inasmuch as magnesium is biodegradable and has a good biocompatibility as well as excellent mechanical properties [1], biodegradable metal scaffolds are mainly made of magnesium and its alloys (such as Mg-Zn, Mg-Y, Mg-Mn, Mg-Al-Zn, Mg-Zn-Mn, Mg-Zn-Mn-Ca) currently [2][3][4][5][6][7][8]. However, these porous scaffolds made of magnesium and its alloys corrode too rapidly in corrosive media because of the high chemical activity of magnesium and large surface areas possessed by the scaffolds.…”
Section: Introductionmentioning
confidence: 99%
“…[18][19][20] Magnesium degrades without toxicity in the body and increases osteoconductivity in vivo, enabling complete bone regeneration at the implant site. 21 In addition, the proliferation and gene expression of osteogenic markers have been shown to be increased in cells exposed to magnesium in vitro. 22 Magnesium silicate (MS) bioceramics have been used in bone tissue engineering because of their osteogenic properties, significant bone-like apatite formation ability, and excellent bioactivity.…”
Section: Introductionmentioning
confidence: 99%
“…The bottle containing scaffold with PBS solution was placed in a shaking water bath (37°C, 80 rpm). The specimens were taken out at the designated point of times (1,3,7,14,21, and 28 days). After wiping off the surface moisture, the specimens were weighed while wet.…”
mentioning
confidence: 99%
“…The elastic modulus of magnesium (45 GPa) is close to that of cortical bone , which will minimize stress shielding effects [10,11]. Among all magnesium materials, the porous magnesium is a research focus for its relatively low elastic modulus and good bone conduction ability [12][13][14].…”