“…Hence, many researchers have prepared CBCCs using pressureless sintering (PS), 25 hydrothermal hot pressing (HHP), 26 hot isostatic pressing (HIP) 27 and spark plasma sintering (SPS) 9,11,[28][29][30][31][32] under no pressure or moderate pressures of 100-200 MPa. 9,27 Martinez et al fabricated cubic boron nitride-tungsten carbide/ cobalt (cBN-WC/Co) composites by HIP.…”