“…In addition, reducing the Pd loading on the Pd/STO-D2 electrode to 0.8 mg, the mass activity for EHDC of 2,4-DCP was further increased to 7.12 min –1 ·g –1 (Figure b). By comparing the mass activity with those reported in the literature under similar conditions, ,,,,,− Pd/STO-D2 was among the most active EHDC catalysts (Figure c). Thus, the use of STO-D as a support greatly helped to reduce the precious Pd required for EHDC of 2,4-DCP.…”