Rapid annealing-transformed, intense-red-emitting Eu-doped ZnGa2O4 nanoparticles with high colour purity, for very-high-resolution display applications

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
11
1

Year Published

2021
2021
2024
2024

Publication Types

Select...
9

Relationship

2
7

Authors

Journals

citations
Cited by 24 publications
(12 citation statements)
references
References 70 publications
0
11
1
Order By: Relevance
“…22,38 Employing a similar combination of MAST and RA, we recently showed that in Eu 3+ :ZnGa 2 O 4 synthesised by MAST, a mere 10 min of RA intensified the red emission, enhancing its color purity while retaining the small particle size. 40 This is in contrast to earlier reports in which Sai et al and Menon et al showed that there is an increase in the crystallite size with the RA temperature for ZnFe 2 O 4 38 and Cr: ZnAl 2 O 4 37 samples. Notably, ZnAl 2 O 4 , like ZnGa 2 O 4 , is transparent to visible-NIR; however, when doped with chromium, grain growth was observed.…”
Section: Introductioncontrasting
confidence: 59%
“…22,38 Employing a similar combination of MAST and RA, we recently showed that in Eu 3+ :ZnGa 2 O 4 synthesised by MAST, a mere 10 min of RA intensified the red emission, enhancing its color purity while retaining the small particle size. 40 This is in contrast to earlier reports in which Sai et al and Menon et al showed that there is an increase in the crystallite size with the RA temperature for ZnFe 2 O 4 38 and Cr: ZnAl 2 O 4 37 samples. Notably, ZnAl 2 O 4 , like ZnGa 2 O 4 , is transparent to visible-NIR; however, when doped with chromium, grain growth was observed.…”
Section: Introductioncontrasting
confidence: 59%
“…4a). The sharp and strong emission bands at 579, 590, 615, 652 and 700 nm correspond to Eu 3+ 5 D 0 → 7 F j transitions where j = 0–4 43–45 and the emission bands at 487, 545, 586 and 621 nm correspond to Tb 3+ 5 D 4 → 7 J j transitions where ( j = 6–3). 46 The variations in the emission intensities of Tb 3+ (545 nm) and Eu 3+ (615 nm) as a function of annealing temperature are given in Fig.…”
Section: Resultsmentioning
confidence: 97%
“…All the bands in the spectra correspond to Eu 3+ and Tb 3+ transitions. 43,44 The variations in emission intensity, as induced by annealing, lead to a shift of the CIE coordinates in the chromaticity diagram from blue to the balanced white light region and from the balanced white light region to the red region (Fig. 4c).…”
Section: Resultsmentioning
confidence: 99%
“…Figure 4(B) shows the decay curve of afterglow and its corresponding second‐order fitting curve of 0.5 at.% Cr:ZnGa 2 O 4 transparent ceramics. The fitting formula was as follows 30 :Inormalt=A1exptτ1+A2exptτ2I(t) is the intensity, τ 1 and τ 2 are the emission attenuation lifetime. A 1 and A 2 are the relative weights.…”
Section: Resultsmentioning
confidence: 99%