“…2a). It has been revealed in previous researches that manufacturing scafold by indirect method results into volumetric shrinkage of scafold after sintering and hence does not serve the required purpose [31,32]. Therefore the volumetric shrinkage needs to be taken care of while designing the ABS mold.…”