2010
DOI: 10.1002/jbm.a.32977
|View full text |Cite|
|
Sign up to set email alerts
|

Repair of calvarial defects in rats by prefabricated, degradable, long fibre composite implants

Abstract: We report results from an initial small animal study designed to provide information on the biocompatibility of a novel biodegradable composite designed for craniomaxillofacial reconstruction. Rat calvarium was chosen as a clinically analogous model, which allowed comparison between experimental groups (PCL alone, PCL/phosphate glass, or PCL/bioglass implants) and control groups (empty defects or bone grafted defects). All animals recovered well from surgery and no clinical complications were observed. Histolo… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
7
0
3

Year Published

2013
2013
2019
2019

Publication Types

Select...
5
1
1

Relationship

0
7

Authors

Journals

citations
Cited by 13 publications
(10 citation statements)
references
References 20 publications
0
7
0
3
Order By: Relevance
“…En el presente estudio, cuando se evaluó el biosilicato cristalino implantado en el alvéolo de ratas ovariectomizadas no se observó degradación o disolución del material en los períodos analizados. Scotchford et al (2011) analizaron la degradación de discos prefabricados que contenían biovidrio implantados en la calota de ratas, demostrando que, tras largos períodos experimentales, es posible encontrar áreas de los discos que sufrieron cambios y deformación, sugiriendo la sustitución del material implantado por tejido del lecho receptor en mayor intensidad a partir de la 8ª semana. Como en el presente trabajo, el período máximo de estudio fue de 28 días, no fue posible hacer comparaciones con los resultados encontrados por estos autores.…”
Section: Discussionunclassified
“…En el presente estudio, cuando se evaluó el biosilicato cristalino implantado en el alvéolo de ratas ovariectomizadas no se observó degradación o disolución del material en los períodos analizados. Scotchford et al (2011) analizaron la degradación de discos prefabricados que contenían biovidrio implantados en la calota de ratas, demostrando que, tras largos períodos experimentales, es posible encontrar áreas de los discos que sufrieron cambios y deformación, sugiriendo la sustitución del material implantado por tejido del lecho receptor en mayor intensidad a partir de la 8ª semana. Como en el presente trabajo, el período máximo de estudio fue de 28 días, no fue posible hacer comparaciones con los resultados encontrados por estos autores.…”
Section: Discussionunclassified
“…This type of model is quite often described in the literature and it is, in a way, acknowledged for this type of in vivo assay. 17 , 18 , 19 , 20 , 21 , 22 , 23 , 24 We used the critical defect model in rat calvaria because it is easy to create, reproduce and the fact that an 8 mm-extension defect would allow us to verify the occurrence of osteoconduction or induction of the material in a standardized and reliable manner.…”
Section: Discussionmentioning
confidence: 99%
“…Como a proposta do fabricante foi inserir um tratamento de superfície nas partículas de fosfato de cálcio que possibilitasse a osteoindução, um modelo de defeito ósseo crítico poderia fornecer informações importantes se a neoformação óssea ocorresse onde ela não seria esperada. Este tipo de modelo é bastante descrito na literatura e está de certa forma consagrado para este tipo de ensaio in vivo (Einhorn, 1999;Cacchioli et al, 2006;Bodde et al, 2008;Messora et al, 2008;Efeoglu et al, 2009;Paulo Ade et al, 2011;Scotchford et al, 2011;Spicer et al, 2012). Utilizamos o modelo de defeito critico em calvária de ratos pela facilidade de confecção, reprodutibilidade e pelo fato de que em 8mm de extensão o defeito permitiria verificar a ocorrência de osteocondução ou indução do material de forma padronizada e confiável.…”
Section: Discussionunclassified
“…Embora se saiba que o tamanho mínimo do defeito em milímetros seja diferente para cada animal, vem sendo defendida e bastante utilizada a produção de defeito circular com 8 milímetros na calvária de ratos Wistar (Einhorn, 1999;Cacchioli et al, 2006;Bodde et al, 2008;Messora et al, 2008;Efeoglu et al, 2009;Paulo Ade et al, 2011;Scotchford et al, 2011;Spicer et al, 2012 Fernandes, 2011).…”
Section: Modelos Animais Para O Estudo De Biomateriaisunclassified