Seawater ageing of low styrene emission resins for marine composites: Mechanical behaviour and nano-indentation studies

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
21
0
5

Year Published

2011
2011
2020
2020

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 37 publications
(28 citation statements)
references
References 8 publications
2
21
0
5
Order By: Relevance
“…It can therefore be observed in figure 8 that hygroscopic ageing did not significantly affect the T g of polyesters (with an average value of 56°C after ageing). Some authors have reported a fall of T g during hygroscopic ageing which could vary from 10°C up to 80°C approximately [31][32][33][34][35]. For the unsaturated polyester resins, T g is expected to decrease considerably beyond 1 % of absorbed water.…”
Section: The Glass-transition Temperature Measurementmentioning
confidence: 99%
“…It can therefore be observed in figure 8 that hygroscopic ageing did not significantly affect the T g of polyesters (with an average value of 56°C after ageing). Some authors have reported a fall of T g during hygroscopic ageing which could vary from 10°C up to 80°C approximately [31][32][33][34][35]. For the unsaturated polyester resins, T g is expected to decrease considerably beyond 1 % of absorbed water.…”
Section: The Glass-transition Temperature Measurementmentioning
confidence: 99%
“…Para los compuestos VEMAT en NaCl, se produce un aumento rápido en la masa del compuesto [Maurin 2009], con una ganancia en peso del 0.20-0.25%, alcanzando posteriormente un plateau [Mouritz 2004] o tendiendo hacia valores inferiores como ocurre en los compuestos VETF donde a su vez la absorción de disolución es inferior a la obtenida en VEMAT. En el caso de que se pérdida de masa, es una evidencia de que se tiene lugar el mecanismo de lixiviación.…”
Section: Análisis De La Variación De Masaunclassified
“…[Hodzic 2001], teniendo en cuenta que la el agua, con un pH ligeramente superior al NaCl provoca mayor nivel de degradación, de igual modo que ocurría en las propiedades mecánicas a escala macro. La degradación en los extremos de la muestra es más evidente, debido a que es la zona más expuesta [Maurin 2009]. …”
Section: Análisis Térmicounclassified