Structure and properties of Fe 3 O 4 films grown on ZnO template via metal organic chemical vapor deposition

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
3
0

Year Published

2016
2016
2022
2022

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 20 publications
(3 citation statements)
references
References 35 publications
0
3
0
Order By: Relevance
“…The binding energy peaks at 711.0 eV and 712.9 eV are attributed to Fe 2þ and Fe 3þ for Fe 2p3/2, respectively. 26 In addition, the binding energy peaks at 1021.7 eV and 1044.9 eV in Fig. 3(d) revealed the existence of Zn.…”
Section: -3mentioning
confidence: 84%
“…The binding energy peaks at 711.0 eV and 712.9 eV are attributed to Fe 2þ and Fe 3þ for Fe 2p3/2, respectively. 26 In addition, the binding energy peaks at 1021.7 eV and 1044.9 eV in Fig. 3(d) revealed the existence of Zn.…”
Section: -3mentioning
confidence: 84%
“…Until recently, the ceramic method was the most widely used [6,7]. Spinels are also obtained by the method of aerosol pyrolysis [8,9]. In this case, salts of transition metals are deposited on a substrate heated to 350-500 о С; when decomposed, they are annealed at the temperature of about 900 о С.…”
Section: Introductionmentioning
confidence: 99%
“…The ferromagnetic (Fe 3 O 4 ) particle has spontaneous magnetization with the A-site moments aligned antiparallel to the B-sites at the temperature below the Curie point (860 K). 12,13) The saturation magnetization is an intrinsic property of ferromagnetic and one of the factors that influences the nature of ferromagnetic materials, which is independent of temperature, particle size, and morphology. At the same time, the preparation process also influences the size and morphology of the nanoparticles.…”