Study of high cycle fatigue of PVD surface-modified austempered ductile iron

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

0
4
0

Year Published

2001
2001
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 26 publications
(8 citation statements)
references
References 10 publications
0
4
0
Order By: Relevance
“…This structure results in an exceptional combination of strength, ductility, wear resistance [2,3] and impact resistance [4,5]. The austempering heat treatment converts ductile iron into ADI, bringing about excellent strength, toughness and fatigue characteristics [6][7][8][9][10][11][12][13][14][15]. This heat treatment cycle involves two steps.…”
Section: Introductionmentioning
confidence: 99%
“…This structure results in an exceptional combination of strength, ductility, wear resistance [2,3] and impact resistance [4,5]. The austempering heat treatment converts ductile iron into ADI, bringing about excellent strength, toughness and fatigue characteristics [6][7][8][9][10][11][12][13][14][15]. This heat treatment cycle involves two steps.…”
Section: Introductionmentioning
confidence: 99%
“…However, studies about PVD coatings applied to ADI are very scarce. All existing references correspond to a single research group and do not reach a dozen [11][12][13][14][15][16][17][18][19][20]. Besides, the results obtained on other metal substrates cannot be forwardly extended to ADI because of the presence of the graphite nodules on ADI microstructure.…”
Section: Introductionmentioning
confidence: 99%
“…Biomaterials should not be reduced while corrosion resistance is improved while coating high corrosion resistance that makes these materials superior [19,20].…”
Section: Introductionmentioning
confidence: 99%