2004
DOI: 10.1016/s0955-2219(03)00565-x
|View full text |Cite
|
Sign up to set email alerts
|

Synthesis and characterisation of LiNi1−x−yCoxAlyO2 cathodes for lithium-ion batteries by the PVA precursor method

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
12
0

Year Published

2004
2004
2024
2024

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 23 publications
(13 citation statements)
references
References 11 publications
1
12
0
Order By: Relevance
“…It is interesting to note that the capacity is retained up to first four cycles with a capacity fade of about 10% at the end of 21 cycles. In addition, the doping of Al 3C lowers the capacity fading to a larger extent [17]. A similar trend was observed by Kalyani et al [12].…”
Section: Resultssupporting
confidence: 80%
“…It is interesting to note that the capacity is retained up to first four cycles with a capacity fade of about 10% at the end of 21 cycles. In addition, the doping of Al 3C lowers the capacity fading to a larger extent [17]. A similar trend was observed by Kalyani et al [12].…”
Section: Resultssupporting
confidence: 80%
“…- = not available.T inlet (°C)T outlet (°C)Other ParametersSpray-Drying Instrument SPRAY-DRYING OF SOLUTIONS A. Spray-drying of aqueous solution of nitrates and/or acetates Duvigneaud et al [145]190150-Buchi mini spray-dryer 190He et al [146]and He et al [148]200-400 mL/hBifluid nozzle 0.2 MPaSD-2500 (Shanghai Triowin Lab Technology Company)Kim et al [152]----Kim et al [187]---SD-1000, Tokyo Rikakikai Co. Ltd, Tokyo, JapanKonstantinov et al [153]190–20090–100-Yamato GA32Li et al [154]---Yamato GB32 pulvis mini-sprayLi et al [156]and Li et al [157]---Buchi mini spray-dryer B-290Li et al [160]300100…”
Section: Table A1mentioning
confidence: 99%
“…However, the high capacity fading on charge-discharge cycling and the low thermal stability in the charged state have inhibited its commercialization. These drawbacks are related to the difficulty in obtaining stoichiometric LiNiO 2 because high temperature treatments have led to the creation of Li 1-x Ni 1+x O 2 , which has a partially disordered cationic distribution at the Li site [3]. Partial substitution for nickel by either a transition or non-transition metal is expected to improve the two dimensional layered structure and the capacity fading upon cycling [4][5][6][7][8][9].…”
Section: Introductionmentioning
confidence: 99%