2017
DOI: 10.1080/15421406.2017.1352420
|View full text |Cite
|
Sign up to set email alerts
|

Synthesis and characterization of UV-curable polyurethane acrylates with PLA and PEG

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2019
2019
2020
2020

Publication Types

Select...
3

Relationship

0
3

Authors

Journals

citations
Cited by 3 publications
(3 citation statements)
references
References 9 publications
0
3
0
Order By: Relevance
“…The subsequently dramatic decompositions occur in the second stage ranging from 250 to 370 °C, which is attributed to the destructions of strong chemical bonds such as urethane bonds. The third stage arranges from 370 to 450 °C, and the weight loss can be ascribed to the decompositions of the rigid groups such as carbamido and benzene ring structures . Here, the corresponding temperatures [inset in Figure (b)] of 5% weight loss ( T 5% ) and maximum weight loss ( T max ) are both used to further discriminate the heat stability properties of PUA resins.…”
Section: Resultsmentioning
confidence: 99%
“…The subsequently dramatic decompositions occur in the second stage ranging from 250 to 370 °C, which is attributed to the destructions of strong chemical bonds such as urethane bonds. The third stage arranges from 370 to 450 °C, and the weight loss can be ascribed to the decompositions of the rigid groups such as carbamido and benzene ring structures . Here, the corresponding temperatures [inset in Figure (b)] of 5% weight loss ( T 5% ) and maximum weight loss ( T max ) are both used to further discriminate the heat stability properties of PUA resins.…”
Section: Resultsmentioning
confidence: 99%
“…There has been a growing interest in the coating and printing industry to develop environmentally friendly coatings or printings, as consumers have become more conscious about environmental issues and more stringent environmental legislations have been implemented in the world (Kim et al , 2017). Moreover, solvent-based raw materials used in coating and printing industry contain organic solvents which pollute atmosphere and lead to severe health problems in humans.…”
Section: Introductionmentioning
confidence: 99%
“…Polyurethanes (PUs) have been commonly employed in adhesives and coating industries. In recent years, water-borne PUs have attracted much interest and are expected to replace their solvent-based counterparts (Kim et al , 2017). Radiation curing technology, such as UV curing system, has some advantages like space saving, energy efficiency, reliable and fast curing compared to thermal systems (El-Molla, 2007; Li et al , 2018).…”
Section: Introductionmentioning